Mending, levelling and smoothing of wall and ceiling surfaces
Surfaces painted with ACRYLCOLOR RELIEF or JUPOL RUSTIKAL
Polishing process of surfaces, which have been painted with relief wall paints, depends on the type of the applied paint.a)
If present paint application is resistant only to dry scrubbing (JUPOL RUSTIKAL or a similar paint was used for painting), then the matter is simple: sprinkle the surface with water or roll it several times using a wet fur roller and thus soften the paint application. Then, remove it using a trowel and wash away any remains with a wet cloth. Afterwards, the dry wall surface
– is either repaired locally (repair only damages – scratches, abrasions, lesions, and similar) with JUBOLIN REPARATUR or JUBOLIN P-25 (the easiest way), or with JUBOLIN or NIVELIN (the more difficult way),
- or entirely polished with JUBOLIN or JUBOLIN P-25 or NIVELIN.
In both cases, coat the cleaned surface with diluted ACRYL EMULSION first (ACRYL EMULSION : water = 1 :1), and apply levelling compound usually in two, but if necessary, in more coats in thickness of 1 to 2 mm. Remove excess compound from the treated surface using a stainless steel smoothing trowel, while trying to smooth the surface as much as possible. Sand the first coat with sandpaper prior to the application of the second one, and the same with the second or the final coat. Grinding can be performed either manually or by machine.
estimation of use of the levelling compound for local repairs (JUBOLIN, REPARATUR, JUBOLIN P-25, JUBOLIN or NIVELIN) is not possible because it depends on the number, size and depth of defects and damages
to polish a m2 of medium rough surface, you will need ~1.5 to 2 kilos of JUBOLIN (manual application) or JUBOLIN P-25 (manual or machine application) or ~1 to 1.5 kilo of NIVELIN (manual application) and ~0.1 kilo of AKRIL EMULSION.
b)
If the surface is painted with washable relief paints or relief paints resistant to wet scrubbing (e.g. ACRYLCOLOR RELIEF), rub them well using a trowel and remove all loose and badly-adhered particles. Then, remove dust from the surface (it is best to wash it). The next phase is smoothing with JUBOLIN or JUBOLIN P-25 or NIVELIN, which is applied in usually two, but if necessary, in more coats in thickness of 1 to 2 mm. Regardless of the manner of application, remove excess compound from the treated surface using a stainless steel smoothing trowel, while trying to smooth the surface as much as possible. Sand the first coat with sandpaper prior to the application of the second one, and the same with the second or the final coat. Grinding can be either manual or performed by a machine.
to polish a m2 of medium rough surface, you will need ~1.5 to 2 kilos of JUBOLIN
(manual application) or JUBOLIN P-25 (manual or machine application)or ~1 to 1.5 kilo of
NIVELIN (manual application)